This is an effective lead-base substitute for Adamant. Defender metal will give excellent service under all shock loads with the possible exception of the bear- ings of some Diesel engines. It has better anti-friction qualities than Adamant but must be poured with care, because Defender does not bond to the shell as easily as Adamant.

Bearing
Metal

Ultimate
Strength
lb. per sq. In.

Yeild
Point
lb. per sq. in.
Brinell
Hardness
Pouring
Range

ADAMANT
Super-Genuine

12,850 8,625 22.8 775-825
degree F
DEFENDER 16,100 7,685 19.5 750-800
degree F
MAGNOLIA
Anti-Friction
18,000 8,975 23.0 750-825
degree F
POWER
Nickel-Genuine
18,500 11,600 32.1 850-925
degree F
PYRAMID 17,850 8,875 24.0 750-1000
degree F
DZL Marine
Nickel-Genuine
17,000 9,510 29.6 850-925
degree F
CP-12
Special Alloy
17,500 9,200 24 850
degree F