Bearing
Metal |
Ultimate
Strength
lb. per sq. In.
|
Yeild
Point
lb. per sq. in. |
Brinell
Hardness |
Pouring
Range |
|
ADAMANT
Super-Genuine
|
12,850 |
8,625 |
22.8 |
775-825
degree F |
| DEFENDER |
16,100 |
7,685 |
19.5 |
750-800
degree F |
MAGNOLIA
Anti-Friction |
18,000 |
8,975 |
23.0 |
750-825
degree F |
POWER
Nickel-Genuine |
18,500 |
11,600 |
32.1 |
850-925
degree F |
| PYRAMID |
17,850 |
8,875 |
24.0 |
750-1000
degree F |
DZL Marine
Nickel-Genuine |
17,000 |
9,510 |
29.6 |
850-925
degree F |
CP-12
Special Alloy |
17,500 |
9,200 |
24 |
850
degree F |